1018

This silicate and cyanide free salt mixture is designed for the electrolytic degreasing and activation of iron, copper, brass, white die-castings and zinc based die-castings.
This product contains chelating agents, which dissolve oxides - that makes the ready degreasing solution insensible against hardness components of the water. Instead of silicates other builders are used to get high dispersing ability.

Process Conditions:
  Working temperature: 20 – 60°C
  Current density: 5-10 A/dm²
  Time of exposition: 0,5-4 min.