Gold R 3N for pen plating

This electrolyte has been especially developed for brush plating. The deposits produced by Gold R are bright and can be used for decorative applications. The colour of the layer is approx. 3N.

Process Conditions:
  Working temperature: 20-30°C
  Voltage: approx. 10 V